There is binder in my recipe. These are the processes I’ve used since this problem arose, some new some the same as always . Ice bath, no ice bath, finish in hot water bath then ice water bath, hot water bath to air dry. In all cases the casings did not adhere to sausage. As you would expect, the pep finished in smoker Shrank more then in pep finished in water bath. The casing on the pep finished in smoker looks like a pair of baggy pants where the hot water bath pep is plump tight fitting but comes off with the bit. this problem was non existent until recently.